Dear All,
 
Can you please let me know what are the addtional CO2 Service requirement for Material Selection and how it effects the Material Selection.
Does this requirement(Additional CO2 Sevice) is only for Sour service or this is a General requirement for Material Selection?
 
This requirement is stated in one of the QP Specification for Material for LP Gas Compressor Package.
 
Hope to see your as usual extended co-operation.
 
Regards
Vino P Varghese
Project QA/QC Manager
Doha-Qatar

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...