Dear all, we want to take batch test qualification for EC 308L MIG welding (1.2MM DIA) .Can we know which tests will be applicable for this? also please send all lthe details( such as thickness of base metal ).We also want to carry out impact @-196C for this .Please share information regarding this. Regards Vinit |
--