7.85gm/cc
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of john clough
Sent: Tuesday, November 16, 2010 9:45 AM
To: materials-welding
Subject: [MW:8287] Specific Gravity
Importance: High
Dear Sirs
How do you calculate the specific gravity in order to calculate the welding consumables?
John
--