As per B31.3, it is not necessary to do the RT for P1 material after PWHT. Regards, P.Mahendran
--- On Mon, 15/11/10, mahendra reddy <mahendra.mog@gmail.com> wrote:
From: mahendra reddy <mahendra.mog@gmail.com> Subject: Re: [MW:8276] PWHT and RT To: materials-welding@googlegroups.com Date: Monday, 15 November, 2010, 11:16 PM
Dear Sager Before is our internal to sure that joint is ok to avoid the 2 times PWHT. After PWHT RT+ mpi is the one which is recordable. if u dont want u can avoid before pwht RT if u r sure that ur welders are perfect there will be no repairs. THX & RGDS M.M.REDDY QA/QC INSPECTOR (WELDING / PIPING) GAS TO LIQUID PROJECT ESCRAVOS - NIGERIA +2347054163177 On Mon, Nov 15, 2010 at 11:50 AM, Sagar QC <sagarqcwelding80@gmail.com> wrote: Hi, I have a doubt regarding PWHT and RT. We are welding P1 Material Pipes which has thickness more than 19mm so we are performing PWHT for the same. But my question is regarding when to take RT? Can we accept the joints which is radiographed before PWHT and MPI after PWHT. Or will we have to perform the RT only after PWHT of the joints? Please advice me regarding this and provide the supporting clause.
Thanks and Regards, Sagar. -- To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/ The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-- -- To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
|
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/ The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment