Tuesday, October 19, 2010

Re: Re: [MW:7640] Change in electrode manufacturer

Hi,
Yes.You can use the existing wps.
 
Thanks & Regards,
 
(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Tue, 10/19/10, krishna <wiqw@rediffmail.com> wrote:

From: krishna <wiqw@rediffmail.com>
Subject: Re: Re: [MW:7638] Change in electrode manufacturer
To: materials-welding@googlegroups.com
Date: Tuesday, October 19, 2010, 12:13 PM


Dear Mr.Karthik,
That means no need to prepare seperate WPS,SHALL WE CONTINUE WITH SAME WPS and use honavar electodes.
thanks,
kk
On Tue, 19 Oct 2010 10:35:32 +0530 wrote
>Hi,
You can use.The brand is a non essential variable.

Thanks & Regards,

(Karthik)
>
>
Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282
>
>--- On Tue, 10/19/10, krishna wrote:
>

>From: krishna
>Subject: [MW:7635] Change in electrode manufacturer
>To: materials-welding@googlegroups.com
>Date: Tuesday, October 19, 2010, 11:15 AM
>
>
Hi frnds,
>Please clarify the below
>
>we have qualified a welding procedure with ESAB E07018 and it is passed we are doing the production welding .
>
>Now we have no stock of ESAB so we are using HONAVAR Electrodes with the same WPS.
>
>Is it acceptable or we have to make another procedure with honavar electordes.
>
>regards,
>kk
>




--
>To post to this group, send email to materials-welding@googlegroups.com
>To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
>For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>






--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...