Dear All
Some companies specification don't allow to change electrode brand or batch, so you have to follow your company specification, in some cases for SMAW if impact tests are required the brand of the electrode can not be changed without further impact tests
Kind Regards
Mahmoud


From: krishna <wiqw@rediffmail.com>
To: materials-welding@googlegroups.com
Sent: Tue, October 19, 2010 9:13:59 AM
Subject: Re: Re: [MW:7638] Change in electrode manufacturer


Dear Mr.Karthik,
That means no need to prepare seperate WPS,SHALL WE CONTINUE WITH SAME WPS and use honavar electodes.
thanks,
kk
On Tue, 19 Oct 2010 10:35:32 +0530 wrote
>Hi,
You can use.The brand is a non essential variable.

Thanks & Regards,

(Karthik)
>
>
Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282
>
>--- On Tue, 10/19/10, krishna wrote:
>

>From: krishna
>Subject: [MW:7635] Change in electrode manufacturer
>To: materials-welding@googlegroups.com
>Date: Tuesday, October 19, 2010, 11:15 AM
>
>
Hi frnds,
>Please clarify the below
>
>we have qualified a welding procedure with ESAB E07018 and it is passed we are doing the production welding .
>
>Now we have no stock of ESAB so we are using HONAVAR Electrodes with the same WPS.
>
>Is it acceptable or we have to make another procedure with honavar electordes.
>
>regards,
>kk
>




--
>To post to this group, send email to materials-welding@googlegroups.com
>To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
>For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>






--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.