Hi,
Yes.But you have to confirm with your customer specification also.Some customer have mentioned about the brand name of electrode to be used for the particular job/project.
 
Thanks & Regards,
 
(karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Tue, 10/19/10, Harikrishnan N S <hari.qaqc@gmail.com> wrote:

From: Harikrishnan N S <hari.qaqc@gmail.com>
Subject: Re: [MW:7639] RE: 7635] Change in electrode manufacturer
To: materials-welding@googlegroups.com
Date: Tuesday, October 19, 2010, 12:30 PM

Dear All

Can you clarify whether this is applicable in situations like Sour Service.

My understanding is that: For Sour Service requirement, because no consumables are established till date, shall qualify the brand, batch and AWS classification. The same brand and batch shall be used in production welding also.

Please correct me if I'm wrong.

Regards

Harikrishnan N S




On Tue, Oct 19, 2010 at 12:05 PM, Ahmad, Aftab <Aftab.Ahmad@omv.com> wrote:

Your question is interesting. As long as the code is concerned, electrodes brands are not essential parameter and it should not require re-qualification of WPS. But some times it happens that with one brand of electrodes some times WPS does not qualify and just by switching from one brand to another brand the same WPS qualifies. It shows that brands play a very important role in qualification of WPS that can be ignored despite the electrodes brands conform to the standard. I would ask forum for their expert opinion in significance of the electrode brands in qualification of the WPS.  

 

Best Wishes

Aftab Ahmad

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of krishna
Sent: Tuesday, October 19, 2010 9:16 AM
To: materials-welding@googlegroups.com
Subject: [MW:7635] Change in electrode manufacturer

 

Hi frnds,
Please clarify the below

we have qualified a welding procedure with ESAB E07018 and it is passed we are doing the production welding .

Now we have no stock of ESAB so we are using HONAVAR Electrodes with the same WPS.

Is it acceptable or we have to make another procedure with honavar electordes.

regards,
kk

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...