Dear Mr Vasu.
 
please refer Electrodes Manufacture recommendation, that stats all your question.
and then your company specification will give more detail regarding consumable control electrode handling procedure etc.
Regards
N.Devan
 

 
On 10/11/10, vasu k <vasuk2577@gmail.com> wrote:
Dear All,

Iam new to piping. I have some basic doubts and i request you to please clarify..

1. In our fab yard, in the evening after the work is finished, the remaining electrodes(E-7018 and E-7018-1) are being kept back in the oven and the entire night the oven will be at 150 deg.
    Will it affect the coating if they r kept for that much time (the entire night)?

2. Do i have to do baking for those electrodes again in the morning?

3. What is the max number of recycling of electrodes?

4. what is the purpose of doing baking till 250 deg ? doesnt the moisture will be removed if we maintain 150 deg i.e  continuously at holding temp?

Regards,

vasu.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Natarajan.Devan
Senior Welding Inspector-AWS
Al Furat Petroleum Co-Syria
Syria Shell Petroleum Development
Tel: 00963 11 6182103 Res
Mobile: 00963 933052385

INDIA: 0091 9840330143 Res.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...