Dear All,
I need your help.I have some material certificates from vendors.I have to review and give feed back to procurement department based on BSEN 10025.But I found that the mill certificates looks like cut and paste from somewhere else.I couldn't find any EN10204 3.1 or 3.2 marking.My client want material based on EN standard but mill certificate showing JIS standard.ChemicaI&mechanical properties,heat number,dimension, are available in the certificate.
1. As per BSEN 10025 what are all the items required in the mill certificate ?
2.Is it mandatory that all mill certificate shall be 3.2 ?
3.Can I accept mill certificate with out BSEN 10025 identification?
Regards,
Limesh
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment