Pl refer electrode manufacturer recommendation

 

Regards

 

M.G.Kattimani

 

-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of vasu k
Sent:
Monday, October 11, 2010 10:48 PM
To: materials-welding@googlegroups.com
Subject: [MW:7486] reg baking

 

Dear All,

Iam new to piping. I have some basic doubts and i request you to please clarify..

1. In our fab yard, in the evening after the work is finished, the remaining electrodes(E-7018 and E-7018-1) are being kept back in the oven and the entire night the oven will be at 150 deg.
    Will it affect the coating if they r kept for that much time (the entire night)?

2. Do i have to do baking for those electrodes again in the morning?

3. What is the max number of recycling of electrodes?

4. what is the purpose of doing baking till 250 deg ? doesnt the moisture will be removed if we maintain 150 deg i.e  continuously at holding temp?

Regards,

vasu.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 
NOTICE - This communication may contain confidential and privileged
information that is for the sole use of the intended recipient. Any viewing,
copying or distribution of, or reliance on this message by unintended
recipients is strictly prohibited. If you have received this message in
error, please notify us immediately by replying to the message and deleting
it from your computer.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...