Re: [MW:7342] difference between E7018 and E7018-1

Adi,
Please see this:
http://www.pirate4x4.com/tech/billavista/PDFs/Excaliber%207018%20rod.pdf,
E 7018-1 has improved low temp impact properties.
Regards,
Shashank Vagal


--- On Wed, 29/9/10, Adi <adinraos@gmail.com> wrote:

From: Adi <adinraos@gmail.com>
Subject: [MW:7267] difference between E7018 and E7018-1
To: "Materials & Welding" <materials-welding@googlegroups.com>
Date: Wednesday, 29 September, 2010, 5:21 PM

Hi everybody

What is difference between E7018 and E7018-1
what is meant by "-1"

Adi

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...