Saturday, October 2, 2010

Re: [MW:7320] RE: 7290] Electrode for cast steel

You can use Lastik 90 from German Gulf to weld the cast stell it is give nice results
Regards
Hani Alfe


From: John Du Plessis <duplessisj@saiw.co.za>
To: materials-welding@googlegroups.com
Sent: Fri, October 1, 2010 8:40:34 AM
Subject: [MW:7298] RE: 7290] Electrode for cast steel

 

 

 

Larry

 

One treats cast steel similar to wrought steel. Match the strength of the cast steel with the strength of the electrode. Depending on carbon equivalent pre and post weld heating might apply.

 

If you have the grade of material I can be more specific.

 

John du Plessis

Technology Manager

 

Tel: +27 (11) 298 2100

Tel: +27 (11) 298 2103 (Direct)

Fax: +27 (11) 836 6014

Mobile:+27  82 883 4970

www.saiw.co.za

 

This email and any files transmitted with it are confidential and may be legally privileged. They are intended solely for the use of the individual or entity to whom they are addressed. Access to this e-mail by anyone else is unauthorised, and any disclosure, copying, distribution or other use of this e-mail is prohibited and may be unlawful. We will not under any circumstances have any responsibility or liability arising out of or in connection with any unauthorised use of this e-mail. If you have received this email in error please notify the sender before deleting it.

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Larry
Sent: 01 October 2010 04:23 AM
To: materials-welding@googlegroups.com
Subject: [MW:7290] Electrode for cast steel

 

Hi,

 

Can anybody suggest a good electrode for cast steel?

 

No code applies, just common welding.

 

 

Thanks in advance.

 

 

 

Cheers,

Larry

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...