Dear Suresh,
Since Welding progression is a non-essential variable as per ASME Sec-IX, there is no need to re-qualify the PQR .
Only you have to qualify welders in downhill position.
Regards
Shadab Alam Ansari
Welding Engineer
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of suresh kochayatu
Sent: Friday, October 01, 2010 10:44 PM
To: materials-welding@googlegroups.com
Subject: [MW:7314] WPS FOR DOWNHILL WELDING
Dear gents,
Could anybody help me for the following concerns,
We have a company approved PQR and WPS for welding P1 to P1material with GTAW process .Now we need to use this WPS for down hill welding. Materials, consumables process are same. According to ASME 1X welding progression is non essential variable for WPS and essential variable for welder qualification.So only welder qualification is enough for using the existing WPS for down hill welding?
Thanks and regards
Suresh
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment