Re: [MW:7155] Copper Slag Abrasive


Hi Srijit ,

only silica sand blasting is banned but copper slag no ban and being
used every where


Muthu Barathi P

Senior Manager QA / QC

AFCONS
On Wed, 22 Sep 2010 18:51:54 +0530 wrote
>Hi everyone,
                    I came across many coating specs which are having
one common sentence " Silica sand and copper slag shall not be used for
blasting".

What is the issue with using copper slag ? What are the dis advantages
of copper slag?

--
- Sreejith Nair-





--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding-
unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-
welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.
>


Dear Sir,





Thanking You,

Honesty is the best Policy

With Warm Regards,

P Muthu Barathi
Mobile No:09967300544

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...