Re: [MW:7142] PWHT PROCDURE

Hi,
Acc.to QW407.1 - noPWHT need seperate PQR.
 
Regards,
 
(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Wed, 9/22/10, KASHKOUSHA <kashkousha1@yahoo.com> wrote:

From: KASHKOUSHA <kashkousha1@yahoo.com>
Subject: [MW:7138] PWHT PROCDURE
To: materials-welding@googlegroups.com
Date: Wednesday, September 22, 2010, 3:23 PM


DEAR ALL
Acc. to ASME IX ,can i use W.P.S. with PWHT  in anther job wihtout  PWHT
pls. your refernce
thanks
H.KASHKOUSHA

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...