Hello,

 

Other than ASME SEC VIII Div1 is there any published LPT acceptance criteria for gas turbine components?

 

Regards,

 

Girish Shejale


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of PREM SHANKARDUTT NAUTIYAL
Sent: Friday, August 27, 2010 8:58 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:6749] acceptance criteria of DPT

 


Hi

If your construction code is ASME Sec VIII Div.1, then refer Mandatory Appendix 8 for LPT acceptance criteria.

The acceptance standards mentioned in ASME Sec VIII Div 1, 2007 edition are:

All surfaces examined shall be free from :
Relevant linear indications ( greater than 1.6mm)
Relevant Rounded indications greater than 5mm.
Four or more relevant rounded indications in a line separated by 1.5mm or less (edge to edge).

Regards

Prem Nautiyal

On Fri, 27 Aug 2010 09:07:43 +0530 wrote
>HI FRIENDS,
CAN ANY BODY TELL ME ABOUT THE ACCEPTANCE CRITERIA OF DPT ?ACCEPTANCE RANGES OF DEFECTS LIKE UNDERCUT,PORE,POROSITY,CRACK,etc.thanks
 
Regards
M.Aslam Khan
QA/QC ENGINEER



--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>


PREM S NAUTIYAL
CELL : 9820313278

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...