Tuesday, September 21, 2010

Re: [MW:7116] PWHT of 4140

Hi,
 
Stress Relief @ 625~640 deg cel, soaking time as per thickness,
 
Yes, it doesn't have P-No. (Need to check with ASME 2010 Edition)
 
Pls consider the history of earlier Heat treatment in as delivery of material
 
Regards,
 
K.Babu
Singapore
 
----- Original Message -----
Sent: Tuesday, September 21, 2010 12:09 AM
Subject: [MW:7113] PWHT of 4140

Dear experts,
                    Can you please tell me how to get the PWHT cycle for 4140? As this material does not have P No. in ASME Sec IX.


regards,
Harish.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...