Re: [MW:7075] PWHT and As welded for flux spec.

As stated in Spec, the flux is tested only after PWHT and properties are assured  only in PWHT condition.  In case you want use the same in As welded condition you  have to contact Manufacturer for its properties in As welded condition. 
 
Regards
 
N.V. PRASAD

On Sat, Sep 18, 2010 at 8:49 AM, Sohil M Mehta <sohilmehta@gmail.com> wrote:
What would be the change in spec if it is in PWHT to As welded for a
particular flux.

eg If flux spec is F7P5XX (PWHT) then what would be in As welded.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...