Monday, September 13, 2010

Re: [MW:6970] Buttering of weld joints

Hi

Buttering thickness exactly not given in AWS D1.1

But still you consider the C2.6.3 section.

Regards,

K.Babu

----- Original Message -----
From: "Engineer Mech" <mengineer010@gmail.com>
To: "Subrata Das" <sdas@pkgroup.org>
Cc: <materials-welding@googlegroups.com>
Sent: Sunday, September 12, 2010 9:05 PM
Subject: [MW:6966] Buttering of weld joints

Could any one says, wats the allowable/acceptable thickness for
buttering?
according to AWS D1.1? Where to refer in AWS D1.1

THANKS

On Jun 12, 11:27 am, "Subrata Das" <s...@pkgroup.org> wrote:
> Dear Sir
>
> Can anyone describe me what is "BUTTERING" stands for in welding joint. If
> it is done before depositing the weld metal on job, is it necessary to
> remove the same by back chipping.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...