Dear Mr,Rajesh
 
Regarding the impact test concept and requirements you can get a brief idea from ASME B 31.3  section 323 (Materials) and table 323.3.1, hope this will guide you.
 
Regards,
 
Murthy.J.N          
 
 
Sun, Sep 12, 2010 at 8:54 AM, Rakesh Jain <rk_jain27@yahoo.com> wrote:

Dear friends,

 

Can anyone explain me the concept of impact testing? how to check if impact testing requirments apply for materials am using? and if impact test requirements are appliacble what are the testing requirments? if i have to use any materials which falls below -29 deg c, impact requirments will apply, am i right?  please guide me.

 

Regards,  


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...