Re: [MW:6960] optimum Heat input

Vanchi,
Thanks.
Please can you provide source for this data?
Best regards,
Shashank Vagal

--- On Sat, 11/9/10, Vanchinath S.A. <vanchinaths@gmail.com> wrote:

From: Vanchinath S.A. <vanchinaths@gmail.com>
Subject: Re: [MW:6956] optimum Heat input
To: materials-welding@googlegroups.com
Date: Saturday, 11 September, 2010, 1:43 PM

control heat input of GTAW and SMAW to 1.6 KJ/mm, FCAW - 2KJ/mm and SAW- 2.5KJmm  max
vanchi

On Sat, Sep 11, 2010 at 10:48 AM, Sreejith.Nair <fizzyshadow@gmail.com> wrote:
Is it possible to predict the optimum heat input ( which can give max. impact value) for a given material considering filler material is of same composition of base metal.


--
- Sreejith Nair-

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...