Re: [MW:6905] WELDING CONSUMABLE FOR SA 240 GR 321

Hi,
 
You can use ER 347+E347-16/17 for ss 321 to ss 321 and you can use ER 309L+E309L-16/17 for SS 321 to SA 516 welding
 

Thanks & Regards
Muhammed Ibrahim PK



On 6 September 2010 09:01, manoj john <manojacgnr@gmail.com> wrote:
Dear all,
 
Please  suggest the welding consumable for SMAW & GTAW to weld SA 240 Gr. 321  + SA 240 Gr 321  and SA 240 GR 321 + SA 516 Gr 70/ SA 105.
 
Thanks & Best Regards.
 
Manoj

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...