If your using electrodes which are vaccum packed, no need of baking. Electrodes are packed in normal packing then you need to follow manufacturers recommendations, code only gives minimum requirements.
 
Regards\
Loni 

On Sat, Sep 4, 2010 at 2:40 PM, Srinivas Engr <srinivas.gmsrini@gmail.com> wrote:
Dear all,

I am in confussion?

What's called hermetically sealed packages?
According ASME section 2 c SFA 5.1, Table A3,
for E 7018, its says 140degree Celsius is enough for backing oven
conditions, when its removed from packages.
but some manafatures says 300-350 celsius.

according to Table A3, we can use after baking in holding oven by 140
celsius & with quivers in site. am i right?

Is it correct or not?

When E7018 is expsoed to air, then only we have to baking to 300 - 350
celsius according table A3.

is any conflict in this? r any wrong in this?

Pl clear me...

Thanks
Srinivas

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...