Sunday, September 5, 2010

RE: [MW:6877] Chloride Content

Hi Kisan

Thanks for your help but I want to select either SS 316 or SS 316 L… So can you guide me up to what limit SS 316 is OK and beyond which its not?

 

Thanks & Regards

Praphulla

praphulla.dp@gmail.com

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Kisan Gamane
Sent: Sunday, September 05, 2010 5:41 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:6873] Chloride Content

 

Dear Praphulla

I think material u can used 316 or 316 L. But a cooling water which will enter inside the plumblene ie. to be cloride contain up to 25 ppm.

On Sat, Sep 4, 2010 at 11:32 PM, Praphulla Phirke <praphulla.dp@gmail.com> wrote:

Dear All, Can someone guide me where I can get the details to select the materials according to chloride content in water?

 

Recent in our project customer has asked us to choose the material as per the chloride content..whether to go for SS 316 or 316L.

 What is the limit for SS 316  & 316 L considering the chloride content in the cooling water?

 

 

Thanks & Regards

Praphulla

praphulla.dp@gmail.com

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.




--

Kisan Gamane

 

सर्वे भवन्तु सुखिनः, सर्वे सन्तु  निरामयः
सर्वे  भद्राणि  पश्यन्तु, मा कश्चिद दुखभाग भवेत्.
May all be happy. May all enjoy health and freedom from disease.
May all have prosperity and good luck. May none suffer or fall on evil days.
++++

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...