Thursday, September 2, 2010

Re: [MW:6827] Required Tests

Be carefully, harmonized standard for the PED (CE marking) is the EN287 of 2004 edition and after.

Fernando ASME AI/ANI



2010/9/1 Karthik <karthik6684@yahoo.com>
Hi,
ISO15614 for Welding Procedure Qualification.
For Welder Qualification it shall be as per EN-287-1.
 
Thanks & Regards,
 
(karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Tue, 8/31/10, Harish Kannepalli <harishkannepalli@gmail.com> wrote:

From: Harish Kannepalli <harishkannepalli@gmail.com>
Subject: Re: [MW:6809] Required Tests
To: materials-welding@googlegroups.com
Date: Tuesday, August 31, 2010, 9:42 PM


you can do as per iso 15614-1 or -2.

2010/8/31 Eng/ Mostafa Kamel Hussein <mkh_200@yahoo.com>
Dear,
I hope to the required tests need for the welder performance qualification (WPQ) according to the EN code and i hope to know the name of this code?
SaSa

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
regards,
Harish.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...