NO!

 

See Essential Variable QW-407.1.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of KASHKOUSHA
Sent: Wednesday, September 22, 2010 3:24 AM
To: materials-welding@googlegroups.com
Subject: [MW:7138] PWHT PROCDURE

 


DEAR ALL

Acc. to ASME IX ,can i use W.P.S. with PWHT  in anther job wihtout  PWHT

pls. your refernce

thanks

H.KASHKOUSHA

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...