Dear All,

I'm going to make some Works inside of a dehydrator (please see attachment), the questions are:

  1. If I cut the angle suports without Couch the shell, do i need an R stamp company for mantain the ASME stamp?
  2. If I cut the angle suports and grinding the angle flush to shell, do i need an R company for mantain the ASME stamp?
  3. For cutting the existents excentric reducers as and Weld others, do i need an R company for mantain the ASME stamp?

 

Please escuse my language, i'm not native speaker (or writer :D )

Thank in advance for your cooperation.

 


 

Date: Sat, 18 Sep 2010 21:53:43 +0530
Subject: Re: [MW:7079] F-No&A-No of ERNiCrMo-3
From: raghurambathula@gmail.com
To: materials-welding@googlegroups.com

For ERNiCrMo-3 Fnumber is 43, please recheck WPS if they have specified some other filler such as NiFeCr-1, NiCrMo-9 falls under F45.
A Numbers are not applicable for non ferrous welds

No such condition as for P number/F Number should be same in Sec IX.

On Sat, Sep 18, 2010 at 6:38 PM, limesh M <limesh78@gmail.com> wrote:
Dear All,
 
I want to prepare a WPS for ,
 
material ASTM B 423 (P No-45).
 
Process - GTAW
Construction Code - ASME B31.3
Welding Code - ASME BPV SEC IX
 
What is the F - No. of ERNiCrMo-3?  43 or 45?One of the  WPS in my hand says 45 !!!
I have reviewed ASME BPV SEC IX QW 432,F-No. section and found that 43.Now I need clarification from experts,which one is correct 43 or 45?
 
What is the A - No. of ERNiCrMo-3? I have reviewed QW 422 A-Numbers section,but couldn't find.
 
Is there any condition that P- no. and F- no. shall be same?
 
Seniors, I need your help on this issue.
 
 
Regards,
 
Limesh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...