[MW:7071] Huey Test and IGC

Dear All,
 
What is Huey test ?
 
Huey test and intergranular corrosion test as per ASTM A262 are same or not ?
 
How we are finding the Intergranular corrosion?
 
What is the acceptance criteria?
 
 
Regards,
 
Limesh

--