Friday, September 17, 2010

[MW:7061] Tube sheet to tube joint

I have WPS qualify for plate( SA 240 TYPE 304 ) can i used for tube sheet ( SA 965 F 304L ) to tube joint with seal weld
& is it mandatory to do mock up for the same.
What percentage of expansion is required for tube ( SA 249 TYPE 304 L ) material
Size- 19.05 OD X 1.951 thk 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...