Tuesday, September 14, 2010

[MW:7010] RE: 6995] Qualitative and Quantitative Testing

Sandesh,

 

            Impact tests measure the energy absorbed in fracturing a metal sample at high velocity and are used to quantify toughness. The crack tip opening displacement test is a fracture mechanics test which can be used to calculate the stress intensity at a sharp crack tip in the tested material as well as critical flaw sizes which will result in unstable fracture. Both tests provide quantitative results, however, the CTOD test requires additional calculations to achieve the desired output (normally a critical stress intensity).

 

Seth Norton


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Sandesh Pandey
Sent: Tuesday, September 14, 2010 5:14 AM
To: materials-welding@googlegroups.com
Subject: [MW:6995] Qualitative and Quantitative Testing

 

Dear All

 

Kindly give us information about Qualitative and Quantitative Testing.
What is the difference between CTOD Test and Impact Test,Which one is Qualitative or Quantitative Testing.
 

Reply as soon as possible.

 

Best Regards

Sandesh Pandey
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...