Monday, September 6, 2010

[MW:6894] solution annealing process details for Pipe fitting.

Dear All
 
Any body can suggest me for solution annealing for Pipe fitting.
Is it necessary for pipe fitting for vacuum application.
if necessary kindly suggest temperature & time required for the same asper thickness.
Fitting material is SA 312 TP 304
Fitting Thickness- appx. 3 mm

--
Kisan Gamane
 
ॐ सर्वे भवन्तु सुखिनः, सर्वे सन्तु  निरामयः
सर्वे  भद्राणि  पश्यन्तु, मा कश्चिद दुखभाग भवेत्.
May all be happy. May all enjoy health and freedom from disease.
May all have prosperity and good luck. May none suffer or fall on evil days.
++++

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...