Hi
It's applicable to castings also for sour service application this inclusion content (Mangnese sulphide inclusion) measurement is a part of inspection.
 
vaithiyanathan
Worleyparsons Arabian industries
Oman.
On Wed, May 12, 2010 at 3:43 PM, Aarpee <ramprasad.chari@gmail.com> wrote:
Dear all,
I would like to know whether micro as per ASTM E45 method D on SA216
Casting can be made applicable?I understand that ASTM E45 method D is
applicable only to the WROUGHT products.Customer expects micro as per
ASTM E45 method D for inclusion morphology on all carbon steels
irrespective of whether it is a casting,forging,plate,pipe,fitting
etc.Your input/experience is welcome.
Regards
Aarpee

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
With Best Regards

B.Vaithiyanathan

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...