Bo,

Can you give more details?
- Process used, welding parameters, overlap of weld-beads?
- 1 layer Ni and 2 layers ER-CuNi? Or 1 layer of both
- What Ni and Fe-content are you looking for?

In the doc attached you will find more details on cladding these alloys ---> page 16 and further

Best regards,

Marco
-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of bo gyi
Sent: 11 May 2010 05:41
To: Materials & Welding
Subject: [MW:5137] Copper Nickel weld overlay

I have encountered that Ni & Fe content are too high for two layers of
ERCuNi overlay to SA106 Gr.B.
When I use ERNi-1 as buffer layer, Ni% much more higher than without
buffer.
Can anyone give me some advice?

Regards,

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...