Dear Member.
 
DNV grade A chemical composition : C 0.21, Mn 2.5, Si 0.35.
 
IS 2062 grade B Chemical composition : C0.20, Mn 1.5, Tensil 410 Mpa, Yield 240Mpa -Equivalent Material is ASTM A36M.
 
Regards
N.Devan


 
On 5/10/10, s.selvam@tebma.com <s.selvam@tebma.com> wrote:
Dear Friends,
 
I want to know what is the different/comparision statement of DNV grade "A" and IS 2062 grade "B" steel plate for chemical and physical properties.
 
Any comparision statement is available? If you have pls forward to my mail.
 

Thanks and Regards,

 

S.Selvam

Asst.Manager (Materials)

Tebma Shipyards Ltd,

Malpe - Udupi

(M) 093416 37012

P Save a tree...please don't print this e-mail unless you really need to


 


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Natarajan.Devan
Senior Welding Inspector
Al Furat Petroleum Co-Syria
Syria Shell Petroleum Development
Tel: 00963 11 6182103 Res
Mobile: 00963 933052385

INDIA: 0091 9840330143 Res.
Mobile: 0091 9884745254

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...