Sunday, May 9, 2010

Re: [MW:5110] A number for alloy 600(UNS N06600)

mahendran,
                   A number is applicable for Ferrous material only not for Non ferrous material hence alloy 600 does not have .Please refer Section IX .
 
vaithiyanathan,
QA Engineer,
WorleyParsons Arabian Industries

On Sat, May 8, 2010 at 11:38 AM, mahendran p <pmahe_79@yahoo.co.in> wrote:
Hi,
    Can anybody tell me what is A - number for the alloy 600(UNS N06600), Filler metal ERNiCr3.
 
Thanks & Regards,
P.Mahendran

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
With Best Regards

B.Vaithiyanathan

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...