Re: [MW:5061] acceptable limit of corrosion in carbon steel plates

Dear Elshan,
                        

Acceptable limits for corrosion  are as follows;

  •  steel; <0.15 mm per year, maximum pit rate is 0.2mm per year
  • Copper; <0.005mm/yr per year, maximum pit rate is 0.02mm per year
  • Stainless steel; 0.005 mm per year, with no pitting

Regards,


Yadav Shiva Chelliya,
Inspection Engineer,
Doha Qatar,
+974-6166465



On Mon, May 3, 2010 at 2:17 PM, Elshan Feyzullayev <elshan_f@hotmail.com> wrote:
Dear friends,

Can somebody give me the standard showing the acceptable limits of corrosions on steel plates?

best regards,
elshan.



Hotmail: Trusted email with powerful SPAM protection. Sign up now.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...