Refer ASME B 31.3 Definitions you will get clear idea. these categories are based on service medium and risk associated with leakage of this service medium.Category M is for any minor leakage will result in fatal or seviere consequences .
Most of Piping coming under Normal Fluid service .
Category D -Fire water lines

Regards,
Vaithiyanathan
QA Engineer
WorleyParsons-Arabian Industries
Oman
On Tue, May 4, 2010 at 10:35 AM, dhinesh gnanadhas <dhineshlhmm@gmail.com> wrote:
Hi

Based on Which criteria the Piping services are being categorised as
Category 'D',  'M', Normal & Sevier Cyclic fluid?

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
With Best Regards

B.Vaithiyanathan

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...