Hi tamar,

Best way to control the distrortion is to control the Heat Input & welding
Sequence.

You can simulate the welding sequence in "Sysweld or Ansys" software if the
part is critical or big structure to find out the best welding sequence.

Rgds,

K.Babu


----- Original Message -----
From: "tamer said" <tamer_bajio@yahoo.com>
To: <materials-welding@googlegroups.com>
Sent: Tuesday, May 04, 2010 3:46 PM
Subject: [MW:5053] destortion control


> Dear all,
> Please I want to know the right way for destortion control, methods and
> applications and any related information regarding this issue.
> Best regards
> Tamer Said
> Kuwait
>
>
>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...