Re: [MW:5046] Hydrotest of Piping System

In general Practice it's allowed to do Hydro test  (1.5or 1.2 times design pressure based on design code ) one time only.Retest due to any failure joints will allow but you can not keep on doing retest rather you have identify the causes of failure.
 
Vaithiyanthan
QA Engineer,
WorleyParsons-Arabian Industries
Oman.

On Tue, May 4, 2010 at 10:03 AM, dhinesh gnanadhas <dhineshlhmm@gmail.com> wrote:
Hi.

If the piping system getting fails in every test. Howmany times we can
do the hydro test for the same piping system?

If we are doing the the hydrotest, we are weakening the pipe material.
So, Howmany times the same system can be allowed to retest?

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
With Best Regards

B.Vaithiyanathan

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...