Hi,
       Let me know your design code whether ASME B 31.4/31.8 then only you can decide on extent of NDT.Since it's a modification work you can check with your client what was the design of code of existing line.
 
 
Regards,
Vaithiyanthan
QA Engineer,
WorleyParsons-Arabian industries
Oman

On Mon, May 3, 2010 at 4:39 PM, daniel iordache <daniel.iordache@gmail.com> wrote:
Hello,
 
Our client asked for a modification and implemetation for 4 new pipeline that will transfer products( goasoil, water, waste water) over the jetty to barge.....
 
Anyone that have a previous project like that can help me with procentage of inspection especiially for RT test ....?
 
regards
 


--
Daniel Iordache
Bureau Veritas - Angola
Mechanical& Welding Surveyor
Mobile Ao: +244921544583
Mobile Ro:   +40721731728
E-Mail:daniel.iordache@ao.bureauveritas.com
      daniel.iordache@gmail.com
         

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
With Best Regards

B.Vaithiyanathan

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...