Hi
There is no such a limitation ; Pls refer clause 3.73/3.74 of API 650 ;
Rgds,
K.Babu
----- Original Message -----From: KASHKOUSHASent: Monday, May 03, 2010 4:45 PMSubject: Re: [MW:5018] PWHT - API 650hi
PWHT in API-650 acc. to .project spec. expect for clean out door is mandatory stress relief
H.KASHKOUSHA
From: dhinesh gnanadhas <dhineshlhmm@gmail.com>
To: Materials & Welding <materials-welding@googlegroups.com>
Sent: Mon, May 3, 2010 10:31:18 AM
Subject: [MW:5015] PWHT - API 650
Dear All,
Can anybody tell me the PWHT requirements as per API 650.
Any thickness limitation is there?
(E.g - As per 31.3. the thickness 19mm & above need to be stress
releived)
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment