As per ASME IX,

only PT & macro etch is required (QW-193). Tear test & strength test
are required by EEMUA publication 143. Sometime client calls those
tests.

On May 12, 12:22 pm, "Bathula Raghuram (Mumbai - PIPING)"
<R.Bath...@ticb.com> wrote:
> When a weld meets the requirements of UW20.4, it is a full strength weld and does not require qualification by shear load testing. You can use a normal groove weld PQR and state on WPS joint configuration as shown in fig UW 20.1.
>
> However Tube to tube sheet strength weld mock up qualification may required if called in contract specifications, in this case you may have to qualify PQR as per QW193
>
> -----Original Message-----
> From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of federico.29
> Sent: Wednesday, May 12, 2010 3:05 AM
> To: Materials & Welding
> Subject: [MW:5147] PQR tests for tube to tube-sheet strenght weld joint - ASME sez.VIII div.1
>
> Dear sirs,
> according to ASME sez.VIII div.1, which tests are required to perform in PQR for a tube to tube-sheet strenght weld joint? in particular tear test is required?
> (please give me the reference of para of ASME sez.VIII div.1) material involved is Carbon Steel: A350 (tube-sheet) and A334 (tube) welding process is GTAW machine thickness involved: 70 mm (tube-sheet) and 2.77 mm (tube) Thank in advance Fede Lau
>
> Filtered by Hosted Filtering
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg athttp://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...