Thursday, May 6, 2010

[MW:5082] selection of filler wire.

Dear all,

1Q. How to select filler wire ?what are the factors to be
considered while selecting a filler wire ?


regards,
ch.srinivasarao.
chsr.2008@gmail .com
chsr@lntecc.com
delhi

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...