[MW:5002] RE: 5001] artificail defect

Welding alloys with wrong consumable and no preheat will often induce cracking.  ie P5 or P9 chrome with E 7018 consumable.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Ali Asghari
Sent: May-01-10 12:05 AM
To: materials-welding@googlegroups.com
Cc: asgharialigl@gmail.com
Subject: [MW:5001] artificail defect

 

Dear All

i want to make a sample with artificial defects.how can i make transverse or longitudunal crack in weld or base metal?

regards

 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...