Skip to main content

[MW:1843] RE: 1841] Re: 1838] Fabricated Stiffeners

Devang,

As per ASME it is no where specified for external pressure design to use
the staggered intermittent weld to fabricate the stiffeners. Hence, in
my opinion it should not be used. You have to meet the required moment
of inertia for the provided section. It is advisable to fabricate the
stiffener with continuous welding only.

Regards

Somesh Kumar Pandey
KBR Energy & Chemicals
79 Anson Road #20-01
Singapore 079906
Office: +65 6210 7459
Fax: +65 6210 7250
Email: Somesh.Kumar@kbr.com


-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of Devang Patel
Sent: March 30, 2009 1:48 PM
To: materials-welding@googlegroups.com
Subject: [MW:1841] Re: 1838] Fabricated Stiffeners


Thanks, Somesh,

Yes, you are write but my question is can we do staggered intermittent
weld
to fabricate the stiffeners?

ASME Sec. VIII Div-1 told about the stiffeners to shell welding only.


Regards,


Devang Patel
Manager Engineering

INOX INDIA Ltd.
Ph :+91-265-3056392-3056100
Fax :+91-265-2333398-2341449
email : devangp@inoxindia.com
www.inoxindia.com

----- Original Message -----
From: "Somesh Kumar Pandey" <Somesh.Kumar@kbr.com>
To: <materials-welding@googlegroups.com>
Sent: Monday, March 30, 2009 10:45 AM
Subject: [MW:1840] RE: 1838] Fabricated Stiffeners

Dear Devang,

Fabricated stiffeners can be used in external pressure design of shell
of
pressure vessel as per ASME Sec. VIII Div.1. You can refer UG -29 , Fig.
UG 29.1 , UG-30 & Fig. UG-30 of ASME Sec. VIII Div.1 for more details on
the acceptable method of attaching stiffener rings

Regards

Somesh Kumar Pandey
KBR Energy & Chemicals
79 Anson Road #20-01
Singapore 079906
Office: +65 6210 7459
Fax: +65 6210 7250
Email: Somesh.Kumar@kbr.com

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of Devang Patel
Sent: March 30, 2009 12:24 PM
To: materials-welding@googlegroups.com
Subject: [MW:1838] Fabricated Stiffeners


can we use fabricated stiffeners in external pressure design of shell of

pressure vessel?

If, yes than please tell, can we use staggered intermittent weld to
fabricate T or Angle?

Please reply.


Regards,


Devang Patel
Manager Engineering

INOX INDIA Ltd.
Ph :+91-265-3056392-3056100
Fax :+91-265-2333398-2341449
email : devangp@inoxindia.com
www.inoxindia.com

This e-mail, including any attached files, may contain confidential and
privileged information for the sole use of the intended recipient. Any
review, use, distribution, or disclosure by others is strictly
prohibited.
If you are not the intended recipient (or authorized to receive
information
for the intended recipient), please contact the sender by reply e-mail
and
delete all copies of this message.


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...