[MW:1741] Re: Closure/ Tie in joints - NDEs as per B31.3

Thanks Ritu raj for you prompt reply.....
Regards
VJv


On Mar 6, 4:28 pm, Rituraj Bose <boser2...@gmail.com> wrote:
> Hi VJV,
> As per Para 345.2.3 (c) of ASME B31.3 (2006 edn.), you can either do
> 100% RT or 100% UT. If Project Specification asks for, you may have to
> do PT or MT after root pass as per Para 344.7, if nothing mentioned in
> Project Specifications, you can go ahead only for 100% RT and you are
> right that no additional requirement is there in B31.3.
> Regards,
> R. Bose
>
> On Mar 5, 10:56 pm, VJ V <veeve...@gmail.com> wrote:
>
>
>
> > Hi All,
>
> > There are a couple of Tie-in/Closure joints to be welded in the
> > project, I am involved right now. No possibility of Leak test/
> > Hydrotest for that joint..
>
> > Project spec is ASME B31.3(100% RT),and
> > I would like to know is there any requirement of UT and cut bevel MT/
> > UT,additional to RT specified by the Code for Closure/ Tie in joints.
>
> > I couldn't see that requirement(cut bevel MT,UT) in B 31.3......Am I
> > right ?
>
> > I have done earlier UT,cut bevel MT additional to RT in other
> > projects,but that was as per project spec.
>
> > Thanks- Hide quoted text -
>
> - Show quoted text -

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...