Skip to main content

[MW:1825] Re: 1814] Re: RT of Duplex Stainless Steel

You should do UT to confirm the indication

Sent from my Verizon Wireless BlackBerry


From: ndion@Acuren.com
Date: Fri, 27 Mar 2009 10:57:22 +0000
To: <materials-welding@googlegroups.com>
Subject: [MW:1822] Re: 1814] Re: RT of Duplex Stainless Steel

There are only three things that will cause white indications, tungsten in the weld, contaminated flux or excessive filler material.

Sent from my Verizon Wireless BlackBerry


From: "Chaitanya Purohit"
Date: Fri, 27 Mar 2009 15:11:21 +0800
To: <materials-welding@googlegroups.com>
Subject: [MW:1820] RE: 1814] Re: RT of Duplex Stainless Steel

Dear (ndion),

 

Thickness : 20mm

 

Method : X- ray

 

Film      : Class 2

 

Screen used : 0.125mm Pb

 

Regards.

 

C. K. Purohit

General Manager - QC

KNM Process Systems Sdn Bhd - Malaysia

 

HP No. : 6016-3376448


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of ndion@Acuren.com
Sent: Friday, March 27, 2009 11:13 AM
To: materials-welding@googlegroups.com
Subject: [MW:1814] Re: RT of Duplex Stainless Steel

 

How thick is the duplex, what film are they using and what source

Sent from my Verizon Wireless BlackBerry


From: "Chaitanya Purohit"
Date: Fri, 27 Mar 2009 11:03:30 +0800
To: <materials-welding@googlegroups.com>
Subject: [MW:1813] RT of Duplex Stainless Steel

Dear All,

 

I am facing problem during NDT (RT) of Duplex St.Steel) . The RT film shows 4-5” long white indication in the weld area. We tried changing the screen but still the same things appear on the film.

 

The welds are welded with SAW process. Generally the porosities are expected if we use SAW welding for Duplex but this indications are strange for me. Does anybody have experienced the same ?

 

Regards.

 

C. K. Purohit



***DISCLAIMER NOTICE ***

"This email and any files transmitted with it is confidential and is intended only for the use of the recepient(s) named above. If you are not the intended recipient, any review, retransmission, dissemination, distribution, printing, copying or use the information contained in this message or any part thereof in other manner is strictly prohibited. If you receive this email in error, please notify the sender immediately by return email and delete the email and any of its attachments. Any personal views or opinions expressed by the sender shall be understood as neither given nor endorsed by KNM or any of the companies within the Group."








***DISCLAIMER NOTICE ***

"This email and any files transmitted with it is confidential and is intended only for the use of the recepient(s) named above. If you are not the intended recipient, any review, retransmission, dissemination, distribution, printing, copying or use the information contained in this message or any part thereof in other manner is strictly prohibited. If you receive this email in error, please notify the sender immediately by return email and delete the email and any of its attachments. Any personal views or opinions expressed by the sender shall be understood as neither given nor endorsed by KNM or any of the companies within the Group."








--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...