Skip to main content

[MW:1810] RE: 1808] Re: Pre heat requirement for split welding procedures from combined PQR.

The min pre heat shall be 32 Deg C in this case. (87-55)

Rgds

raj

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of ARI
Sent: Thursday, March 26, 2009 4:03 PM
To: materials-welding@googlegroups.com
Subject: [MW:1808] Re: Pre heat requirement for split welding procedures from combined PQR.

 

Dear Ibrahim,

 

You should specify the thickness of the Original PQR and the current thickness of the job, which you intended to utilize FCAW. Based on which only, the experts can respond!

 

regards,

 

On 3/26/09, Muhammed Ibrahim <ibratech@gmail.com> wrote:

Hi friends,

 

I would like to clarify one important thing about preheat. My PQR is qualified with SMAW+FCAW. When I start the welding I preheated to 24 degree C. After root and hot pass compleated with SMAW before starting FCAW the plate temperature is 87 degreeC. If I split this PQR to make a WPS only for FCAW, Is it required to preheat the plate to 87 degree C or can I give 24 degree celcius as preheated in the starting of PQR test coupon?. Your response will be highly appreciated.

 

The AI insisting to put preheat of 87 degree shall be considered when we split the PQR for FCAW because when FCAW process starts the temperature of the plate to be considered as the preheat temperature (87 degreeC).


Thanks & Regards
Muhammed Ibrahim PK
 

<br


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...