[MW:1508] Re: Resistance welding testing lab-Reg

Mettalurgical service, ghatkopar, mumbai
tel- 02-25000240/ 41
Contact:- Mr. patel/ dipen

Regards,
Rupesh Jambhale
HDOlL Mumbai

On Wed, Feb 4, 2009 at 4:06 PM, kums <kums@godrej.com> wrote:
>
> Can anyone tell us the Testing Lab in Mumbai which can do testing of spot
> welded samples.
> tests like Shear test, Peel test,...
>
> Regards
> B.Kumaran
> =======================================================================
> Godrej is now just a call away. Dial our 24 hour toll free number,
> 1-800-225511 for all your queries about our products, prices, dealers
> and service. We will be glad to be of assistance to you.
>
> * Toll free number available in Ahmedabad, Bangalore, Chennai, Delhi, Hyderabad,
> Kolkata, Lucknow, Mumbai, and Pune
>
> " Visit our website - http://www.godrej.com "
> =======================================================================
>
>
>
>
> >
>

--
Regards,

RUPESH A JAMBHALE.

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...