Hello Pravin

Cast iron is one of the difficult metals to weld. Grey cast irons are weldable subject to the original manufacturing process and grades involved. White cast irons are Unwedable. It's important to know what's the grade involved. Welding cast iron is typically a repair weld. Qualifying ASME Sec-IX procedures as like new fabrication  is quite difficult. One may have to settle with reduced angle of bending in "Guided Bend Test". Some resources are attached for guidance.

Usually E-Ni-CI (99% Nickel) or ENiFe-CI(55%Ni) SMAW electrodes or GMAW fillers of equivalent composition are available for the consumable manufacturers.

If you want to know the subject well, get hold of this AWS publication.

Thanks.

 

P.Goswami.P.Eng, IWE.

Independent  & Consulting Welding & Metallurgical Specialist

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@rogers.com,pradip.goswami@gmail.com

Cell/Whasapp:1-905-9793232

 

https://www.lincolnelectric.com/en-us/support/welding-how-to/Pages/welding-cast-iron-detail.aspx

 

 

From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> On Behalf Of Pravin Poornachandran
Sent: November 2, 2020 9:29 PM
To: 'Bijay' via Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:31689] Cast iron to mild steel

 

Dear Expert, 

 

Good day.

 

I have to weld cast iron to mild steel.

What would be the suitable filler rod to use? 

 

Also is there any specific parameter or welding condition I have to follow since cast iron is difficult to weld. 

 

Example any specific heat treatment or post heating before welding? 

 

Kindly advice.

 

Best regards,

Pravin 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADDyn7eaVq1UvD%2BgBxN8BiwjvxLoa4MSduXQisFPpOo4fRfStA%40mail.gmail.com.


Virus-free. www.avg.com

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...